Hi everyone, I want to determine the size of steel ball, according to the equation of Bond and the equation work index: W=WI* (10/√P80 -10/√F80), for calculating Wi, I need to konw the W(work input,kwh/metric ton), so how can I obtain the work input ? my grinder see the photo, constant speed.
thank you